‘杭州20G锅炉管、杭州20G厚壁锅炉管’杭州20G大口径锅炉管‘13820527166
20G锅炉管化学成分、机械性能 :
标准
|
钢级
|
化学成分(%)
|
C
|
Mn
|
Si
|
V
|
Cr
|
Mo
|
P.S
|
GB5310
|
20G
|
0.17~0.24
|
0.35~0.65
|
0.17~0.37
|
/
|
/
|
/
|
≤ 0.030
|
25MnG
|
0.22~0.30
|
0.70~1.00
|
0.17~0.37
|
/
|
/
|
/
|
≤ 0.030
|
15MoG
|
0.12~0.20
|
0.40~0.80
|
0.17~0.37
|
/
|
/
|
0.25~0.35
|
≤ 0.030
|
15CrMoG
|
0.12~0.18
|
0.40~0.70
|
0.17~0.37
|
/
|
0.80~1.10
|
0.40~0.55
|
≤ 0.030
|
12Cr2MoG
|
0.08~0.15
|
0.40~0.70
|
≤ 0.50
|
/
|
2.00~2.50
|
0.90~1.20
|
≤ 0.030
|
12Cr1MoVG
|
0.08~0.15
|
0.40~0.70
|
0.17~0.37
|
0.15~0.30
|
0.90~1.20
|
0.25~0.35
|
≤ 0.030
|
机械性能
|
抗拉强度 (MPa)
|
屈服强度 (MPa)
|
伸长率(%)
|
20G
|
410~550
|
≥ 245
|
≥ 24
|
25MnG
|
≥ 415
|
≥ 240
|
≥ 22
|
15MoG
|
450~600
|
≥ 270
|
≥ 22
|
15CrMoG
|
440~640
|
≥ 235
|
≥ 21
|
12Cr2MoG
|
450~600
|
≥ 280
|
≥ 20
|
12Cr1MoVG
|
470~640
|
≥ 255
|
≥ 21
|